Waspaloy
Chemical composition in wt.%*
Waspaloy
| C | Mn | Si | P | S | Cr | Co | Mo | Ti | Al | B | Fe | Cu | Ni | other |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 0.02 | 1.00 | 0.75 | 0.03 | 0.03 | 18.0 - 21.0 | 12.0 - 15.0 | 3.50 - 5.00 | 2.75 - 3.25 | 1.20 - 1.60 | 0.003 - 0.01 | 2.00 | 0.50 | Bal. | Zr:0,02-0,12 |
| C | 0.02 |
| Mn | 1.00 |
| Si | 0.75 |
| P | 0.03 |
| S | 0.03 |
| Cr | 18.0 - 21.0 |
| Co | 12.0 - 15.0 |
| Mo | 3.50 - 5.00 |
| Ti | 2.75 - 3.25 |
| Al | 1.20 - 1.60 |
| B | 0.003 - 0.01 |
| Fe | 2.00 |
| Cu | 0.50 |
| Ni | Bal. |
| other | Zr:0,02-0,12 |
* unless otherwise stated, these are the maximum values.
Product forms
- Strip
- Plate
- Bars
- Wire
Specifications
| AMS | ASTM | Others | |
|---|---|---|---|
| Strip | AMS 5544 | ||
| Plate | AMS 5544 | ||
| Bar | AMS 5706, AMS 5707, AMS 5708, AMS 5709 | ||
| Wire | AMS 5828 | ||
| Tube | AMS 5586 |
Physical and mechanical Properties
| Density | 8.19 g/cm³ | 0,296 lb/in³ | |
| Mill annealed as shipped | ||
| Strip | Wire | |
| Tensile strength | Max. 1100 MPa (160 ksi) | Max. 1100 MPa (160 ksi) |
| Annealed and aged | ||
| Strip | Wire | |
| Heat treatment | Stabilization 1550°F (845°C) Age 1400°F (760°C) Or per specifications | Stabilization 1550°F (845°C) Age 1400°F (760°C) Or per specifications |
| Tensile strength | Max 1172 MPa (170 ksi) | Min 1103 Mpa (160 ksi ) |
| as shipped Spring temper | ||
| Strip | Wire | |
| Tensile strength | Max. 1379 MPa (200 ksi) | Min. 1379 MPa (200 ksi) |
| Density | 8.19 g/cm³ | 0,296 lb/in³ | |
| Strip, Mill annealed as shipped | ||
| Zugfestigkeit | Max. 1100 MPa (160 ksi) | |
| Strip, Annealed and aged | ||
| Wärmebehandlung | Stabilization 1550°F (845°C) Age 1400°F (760°C) Or per specifications | |
| Zugfestigkeit | Max 1172 MPa (170 ksi) | |
| Strip, as shipped Spring temper | ||
| Zugfestigkeit | Max. 1379 MPa (200 ksi) | |
| Wire, Mill annealed as shipped | ||
| Zugfestigkeit | Max. 1100 MPa (160 ksi) | |
| Wire, Annealed and aged | ||
| Wärmebehandlung | Stabilization 1550°F (845°C) Age 1400°F (760°C) Or per specifications | |
| Zugfestigkeit | Min 1103 Mpa (160 ksi ) | |
| Wire, as shipped Spring temper | ||
| Zugfestigkeit | Min. 1379 MPa (200 ksi) | |
The information in our data sheets is a rough overview and does not claim to be complete. They correspond to the current state of the art. No warranty is assumed.
You can find further Nickel-alloys in our product range.