Alloy K500
Chemical composition in wt.%*
Alloy K500
| C | Mn | Si | S | Ti | Al | Fe | Cu | Ni | other |
|---|---|---|---|---|---|---|---|---|---|
| 0.18 | 1.50 | 0.50 | 0.01 | 0.35 - 0.85 | 2.30 - 3.15 | 2.00 | 27.0 - 33.0 | min. 63.0 |
| C | 0.18 |
| Mn | 1.50 |
| Si | 0.50 |
| S | 0.01 |
| Ti | 0.35 - 0.85 |
| Al | 2.30 - 3.15 |
| Fe | 2.00 |
| Cu | 27.0 - 33.0 |
| Ni | min. 63.0 |
| other |
* unless otherwise stated, these are the maximum values.
Product forms
- Bars
- Wire
Specifications
| AMS | ASTM | Others | |
|---|---|---|---|
| Bar | AMS 4676 | ASTM B865 | NACE MR0175 (ISO 15156-3) |
| Wire | AMS 4676 | ASTM B164, ASTM B865 | NACE MR0175 (ISO 15156-3) |
Physical and mechanical Properties
| Density | 8.44 g/cm³ | 0,305 lb/in³ |
| Mill annealed as shipped | |
| Wire | |
| Heat treatment | 870°C (1600°F) |
| Tensile strength | 550-760 MPa (80-110 ksi) |
| Operating temperature | -184°C bis 232°C (-300°F bis 450°F) |
| Density | 8.44 g/cm³ | 0,305 lb/in³ |
| Wire, Mill annealed as shipped | |
| Wärmebehandlung | 870°C (1600°F) |
| Zugfestigkeit | 550-760 MPa (80-110 ksi) |
| Betriebstemperatur | -184°C bis 232°C (-300°F bis 450°F) |
Do you still have questions or is one of your requirements not listed in our data sheet? Would you simply like to receive a quotation for your needs or project?
No problem!
Send us your request by e-mail to info@hightechalloys.de or contact us by phone at +49 (0) 2103 78981-0.
The information in our data sheets is a rough overview and does not claim to be complete. They correspond to the current state of the art. No warranty is assumed.